By topbobster - 1/6/2014 1:02:33 PM
Hello, I see that your Coating Resin can be used as a laminating resin - for me the positive of this is you state your coating resin "is pure" and can be used on top of previously fully/partly cured coating resin hence removing the need for sanding in between.....
Yet you recomend EL2 Laminating resin - positives for me being the different different slow/fast hardners that can be mixed etc.
Of course I want the best of both worlds so my question is: Does EL2 Laminating resin need to be sanded between layers to keep the mechanical properties and stop delamintion?
I have an upcoming project that will only allow the gradual addition of pieces of fibreglass etc. and being winter I will be working in the house therefore excluding the chance of using Polyester resin.
Regards, Rob
|
By topbobster - 1/6/2014 4:40:57 PM
thanks
|
|