· Elastic Modulus in X: 181 GPa
· ElasticModulus in Y: 181 GPa
· Elastic Modulus in Z: 10.3 GPa
· Poisson in XY: 0.28
· Poisson in YZ:
· Poisson in XZ:
· Shear Modulus in XY: 181 GPa
· Shear Modulus in YZ:
· Shear Modulus in XZ:
· Mass Density: 1600 kg/m³
· Tensile Strenght in X: 1500 Mpa
· Tensile Strenght in Y: 1500 Mpa
· Compressive Strenght in X: 1500 Mpa
· Compressive Strenght in Y: 1500 Mpa
· Yield Strength:
The values that are already filled in are values that i found somewhere. I don't know if they are correct. I hope someone can help me with this.
T