Talk Composites - The Forum for Advanced Composites

Vacuum film

http://www.talkcomposites.com/Topic8687.aspx

By MattByrne - 12/4/2013 10:41:16 AM

Anyone know where I can get high temperature vacuum film? I need it to go to at least 260 degrees, preferably more like 280 or 300
By ChrisR - 12/5/2013 9:57:36 AM

PM sent but that is VERY hot!