By Marco - 11/22/2013 10:19:56 AM
My name is Marco and i'm from tiny Luxembourg. I registered on this forum to get some help with a project i am currently working and to know what products i will be needing from the easycomposite store in order to get my part made. Now this is the first time i will be using fibreglass or carbon fibre so bare with me.
About my project then, I want to build an enclosed airbox for my supercharged GTI6 as the standard setup is not very efficient to say the least. So i drew the part using sketchup and then made a 1 to 1 dummy out of cardboard. This part will be sitting in the enginebay where temperatures will be above the 70°C mark. I am thinking of making the box from Fibreglass and eventually to use carbon fibre lamination to give it a nice look.
Here are some pics of what i have so far:
Sketchup


 You will notice the top of the box is open i am planing on using a 1mm ?wet? carbon sheet to blank it of as i still need to have access to the airfilter every now and then.
Cardboard dummy

I have watched quite some youtube videos on how to work fibreglass and/or Cf, but i just dont know how to make the initial fibreglass box. Do you guys think i can use the cardboard dummy and start to put FG cloth and resin on it? ALso can anyone make me some kind of shopping list of what will be needed from the shop as i really don't know the differences between all the resins, epoxy etc. is.
Any help and input will be greatly appreciated, thank you in advance Cheers
|
By Marco - 11/27/2013 8:58:49 PM
Dravis thank you very much for your reply, i was starting to lose hope anyone would even care 
The box will be subjected to vacuum an should, essentially prevent the filter from sucking the hot air from the engine bay once the engine is up to temperature. Due to my little knowledge of working with composites making the box from a 2 piece mould seems way to complex. As said the main structure is supposed to be made out of fibre glass an afterwards laminated with carbon to give it a nice look. Also this is going to be a one of.
What do you mean by core material? I'll upload some more pics of the setup as it is now to give you a better idea of what i am trying to accomplish.