By Lloyd - 11/12/2013 7:55:43 AM
Hi,
I have just done my first vacuum bagging using EL2 epoxy laminating resin with the slow hardener, my question is how long do you need to leave the vacuum pump running, after the laminate as gelled or dos it need to fully cure?
|
By Warren (Staff) - 11/14/2013 2:11:38 PM
As with infusion, if the bag has no leaks, no need for the pump to be on.
|
|