By philiplardner - 10/22/2013 5:27:38 PM
Hi,
I have a large, thin (1 and 2 layers of CF cloth), complex shape to infuse in a rather flexible mold. I have successfully infused one piece already but found the task of removing the peel ply and resin flow mesh after curing to be very difficult, and came close to damaging the this (2 layer) carbon part before removing it from the mold. I have to infuse a number of equally large parts that consist of only a single layer of carbon cloth and I am pretty sure they will not survive removing the peel ply and mesh layers.
Can I use perforated film instead of peel ply beneath the resin transfer mesh? I don't need the peel ply finish anyway?
Thanks,
Phil.
|
By philiplardner - 10/24/2013 11:09:50 AM
Thanks guys - that's much appreciated advice. I'll knock up a couple of test pieces using this method before I try the large, thin production parts.