From what I've been reading gel-coating and clear coating achieve pretty much the same thing. Is there any advantage of one over the other? Also for gel-coating will a regular spray gun do the trick or is it necessary to use a gel cup gun? Thanks!
By Leew
-
11/5/2013 8:15:54 AM
baja_patient (20/10/2013)
full face mask.
I seem to remember someone telling me that you need an air fed mask to spray gelcoat and that a cartridge mask is not sufficient, is that true?