Hello,
I'm making 2 B-Pillar for my car using the uni-mould system followed by laminating it.
The two moulds were made right without any issues.
Today I tried to laminate them, but when i'm going to put the first layer of resin, it happens that in some parts goes away.
I've used 4 layer of Easy lease.
How can I avoid this?
Thank you very much
By Golfer
-
10/24/2013 12:38:01 PM
Tried to do another part yesterday evening.
the white thing appears when I work constantly the resin.