By aseem - 10/16/2013 10:18:13 PM
I need to make a heat shield to protect the bumper and other parts from muffler heat. The current shield on my car is made of thin aluminium. Can I use aramid alone or together with carbon fiber to make such a piece?
|
By Warren (Staff) - 10/18/2013 12:25:57 PM
As said, its not a problem with the fibres, be it carbon or aramid, but a function of resin TG. You realistically need to measure what the temperature gets upto then decide what to do from there.
|
|