Hi and welcome to the forum Chris
Thanks for the tips and hints! while making the video I've noticed my mistake by not defrosting it before opening the bag.
I didn't know you had to wear gloves while cutting the prepreg without direct contact with the epoxy and so on, I'll keep that in mind for my future video's and let everyone know it's important to do so, because I always try, and think it's very important, to work as safe as possible with those composite materials!