By cpkielycua - 10/6/2013 10:02:53 AM
The cardboard tube the surface layer is shipped on has a normal but relatively small diameter. When unrolling the surface layer, the prepreg is 'used to' being wound around the tube, which causes wrinkles in the carbon/epoxy matrix when unrolled. This negatively effects the finished product. Is there a technique to unrolling the surface layer so it does not wrinkle?Thanks!
|
|