By BoostSamurai - 10/1/2013 3:43:53 PM
Hey guys, I'm about to buy my first ever FG/CF supplies.
I've found a local supplier (because shipping chemicals OS is $$$$ and a big NO NO) and have made a list of what I think I'll need to get started, both in terms of FG mould & CF part making. In the future, I will be getting my composite fabric requirements from EC though 
Could I please trouble you guys to take a look over my list and let me know if there's anything else you think would be essential for a start up and or anything I probably don't need that I have included in my list.
Supplies List- 105 West System Epoxy Resin 1 ltr
- 206 Slow Hardener 800 ml
- PVA Release - 1kg (blue)
- Demoulding Wax 400gm
- Respirator Kit A1B1E1K1-P2 - Ammonia
- Safety Goggles
- Acetone 5 ltr
- Isopropyl Alcohol 99%
- Catalyst for Tooling Gelcoat 500ml
- Tooling Gelcoat 1 kg
- Catalyst - 100ml MEKP
- Polyester Resin for Fibreglass Laminating 1kg
- Plasticene Light Beige Modelling Clay 4kg
- Mixing Sticks
- Paint Brushes
- Carbon Fibre fabric 2x2 twill 198gms
- Fibreglass Cloth 130gm
- Fiberglass Roller 12mmx70mm
Brand/product selection is limited, but this is what I have to work with.
With the above supplies, I hope to produce some simple wet layup CF parts which, when sold, will enable me to acquire enough funds to move forward to an infusion setup.
Thanks in advance
|
By BoostSamurai - 10/2/2013 1:05:10 PM
Thanks for that. I guess I'll have to have a chat with my supplier to see what they have available that is compatible.
|
|