By Johnny - 9/25/2013 10:40:59 PM
Hello, do you have any resin(or equivalent) that takes 2-5 hours to cure?
|
By Dravis - 9/30/2013 10:01:49 PM
Hi Johnny,
Do you mean "Pot-life" i.e. the time you have available to work with the resin?
That is normally found in the information on the product, and dependant on the hardener.
That can be extended if you can work in cooler temperatures, but you will have a higher viscosity too.
"Curing time" is a bit difficult to be precise about, depending of how one defines "cured"...
|
|