By Jozi - 9/19/2013 8:41:29 PM

Is there anyway to prevent the weave distorting? My first attempt I found that laying the cloth cause the weave to distort, wether this was because it was snagging on sticky resin in the mould or from coating the weave with a brush I'm not sure.

There must be a way though to keep the fibres together a little better, I find it quite a fragile material to work with. Could I take 2 layers of cloth and stick them together with resin so it's a bit more durable?

Basically I have some area's where the weave distorted, I'll try get some images up.
By FLD - 9/20/2013 10:11:48 PM

Try using pro-finish.  This is exactly what its intended use is I believe.