By TomDesign - 9/10/2013 5:14:26 PM

They say after they wrap part carbon surface can not be scracted, also burn also not affect also 3 years protection and service. 

That is not real for me! so what resin can hold that or material for me that is space and others who asked.http://www.talkcomposites.com/Uploads/Images/ee3ac576-35b2-4611-9265-5c32.jpghttp://www.talkcomposites.com/Uploads/Images/af3b8970-593d-4af7-ac21-5a30.jpg
By carboncactus - 9/12/2013 5:19:28 PM

Dravis (12/09/2013)

I have never had anyone, customer or not, ask about scratches, or if the skinned parts were more flammable than the original plastic parts ...