Hi allas the title realy, in the instruction guide it states post curing of the mould is not essential if using for normal ambient use but for in mould post curing + pre-preg is it required
is it absolutely essential?
I ask as I dont realy have the ability at the minute to post cure at the temperature for the instructed time length etc, 60 degrees for 10 hours + so on
I can do it for 60 degrees but only 2 hours at a time + it would cool down betwern each time
would this be ok? Has it got to be as per the guide? Is it 100% required?
Thanks in advance for the help
jamea