By japcarmaniac - 2/20/2012 7:17:02 PM

can easy lease be used on a plug to make a mould? and not just for pulling from a mould.
By Joe - 2/21/2012 4:01:31 PM

Hi,

When making a mold, i just use wax and never PVA. But wax amount is at around 10 coats. I never ever had a problem releasing mold from plug.

I always felt that PVA could not be polished so it would leave inprints on the mold, thats why i dont use that.

I dont say thats the right way to proceed, but I never had a problem.