Hello to everyone, as you will see I am new to site and are just getting started ' please if anyone can advise on my project I would be grateful. I am making a carbon fibre sleeve for my eghaust on my motorcycle and I have made mandrel part replica of my eghaust to rap the carbon fibre around and so on, the bit im stuck on is how do I do a neet seem joint where the end of the carbon sheet meets the other , I could overlap it but I am after the look of if two sheets but up to each other ......Please any help
|
By Icet - 9/8/2013 7:20:53 PM
Thank you my friend , I like the idea with pizza cutter seems like that would be a neat finish just what im after ' I'll let you know how I go thanks once again.
|
|