I do get the occasional strange request at carbonfibreworks, this one is for a mask to use at a masked ball, one layer of 450g carbon made with epoxy (wet lay vac bag) and a few coats of clear . All materials from Easy Composites.
Chris
www.carbonfibreworks.co.uk

By Airship-Jim - 8/30/2013 1:41:39 AM

wozza (29/08/2013)
Airship-Jim (29/08/2013)
Love the mask you have done there Chris, excellent finish on it too.

Not surprised that there can be so many unusual requests for work for you pros out there, and I don't think you will have any problems doing a toilet seat for someone warren, after all the shape is "bog-standard" ... sorry for the pun ... ;-D

Jim




SmileSmile At first I admit to being a little peeeeeeed off with the request but now I have done some research into what they sell for I think it may be worth making some moulds. Sorry for the "counter pun" but I could not resist Smile

Warren


I had a look on the internet too, and they sell for a good price £180 to £500 for standard shapes, still it could be a risky business that could go down the pan ! (drum-roll, cymbal).

Jim