By garethpj - 8/28/2013 2:43:42 PM

Greetings from South Africa

Please will you be so kind as to let me know if your Aluminium Honeycomb is suitable to be used in the beds of laser engraving machines?

The bed size of our laser is 52 x 50 inches and the honeycomb has a cell size of about 7mm and is 1 inch thick

Also do you have something called 1” aluminum ecolite which is a square grid

Many thanks
Cheers

Gareth
By Warren (Staff) - 8/28/2013 4:53:19 PM

Hi, we do not stock ecolite.

However, we have plenty of customers using our honeycomb on thier laser beds.  The closest match to your size is our 6.4mm (1/4) Aluminium Honeycomb which is available in 2 sheet sizes and 3 thicknesses.