By karlfranz - 8/25/2013 7:13:13 AM
I was concerned with stirring the basecoat prior to combining it with the hardener because I didn't want to introduce additional bubbles. However, the coat didn't look fully black, it was more translucent than I thought it would be. Is this normal, or am I doing something wrong?
|
By Warren (Staff) - 8/27/2013 12:15:00 PM
Sometimes it is possible for the pigment to settle slightly so gentle stirring is recommended.
|
|