Hi guys,
I've got a bit of a personal project for a family member which involves casting from their knee down to make a mould for a carbon part.
I've watched all the casting vids here and feel confident about the theory but haven't been able to find casting info for half a leg. Does anyone have any experience in this? The plan is to cast in algenate. Does the foot flex enough to get it out without having to split the mould?
Thanks