By GTE-JOHN - 8/4/2013 1:32:21 PM

Hi guys, I am wanting to make a mould of my bonnet for resin infusion but I am a bit stuck trying to figure out where to position the corrugated sign board for the flages on the front edge, as you can see the front edge of the bonnet curves down then the bottom edge kicks back towards the engine, also the side edges of the bonnet have a recessed swage line which I fear may also make the mould lock to it, any help/advice would be great



By GTE-JOHN - 8/5/2013 11:20:24 PM

Thanks for the reply Warren, those details are not important i guess, I could flush the swage line on the sides of the bonnet with filleting wax?? And also trim the front lip so it's a slim edge like on most modern bonnets & also fill the gap between the inner & outer skins with wax again when it comes to doing the inner frame