By armando - 7/21/2013 9:26:29 AM
Hi I'm interesting to experiment with fishing rod blank making, using carbon fiber , have anybody got idea about what type of woven I need to used? Is any web or document on line?or book which relevant info about , I'll appreciated ,the help |
By Warren (Staff) - 7/23/2013 10:54:05 AM
Most tubes like that are made by a roll wrapping technique around a metal mandrel using pre-preg carbon fibres, often Uni-directional pre-pregs at different orientations.
You can do it wet lay then consolidate with a Composites High Shrink Tape before letting it cure.