I have been lucky enough to be involved in the restoration of a BRM P154 Can-Am car as raced by Pedro Rodriguez in the last 3 races of the 1970 season.There was no bodywork with the car but the customer has some of the original moulds, however they have been stored outside since the late 70's and are in a pretty poor state. I have been restoring/replacing the moulds and today I pulled the two doors. Pretty happy with the results given the condition of the moulds. So now it's on to the big bits, nose section next.
Warren