By chemie29 - 6/30/2013 9:02:50 AM

Hi eveybody! is there any limit in shape and size when C.N.C. a piece of PS foam? Mine has a triangular profile with no constant section and is no big (50 cm long by 3 cm wide). I need to use it as a core in part production and I think it is easier than make a PUR foam casting. Thanks
By chemie29 - 7/3/2013 4:00:10 PM

Which would be the recommended density?