By japcarmaniac - 2/12/2012 12:39:58 PM

i seen this today http://nr11.biz/blogfest/?p=25  and have seen many others like it but how do you take parts from it as they never seem to show you how they do it. im just wondering how they join the two halfs.
By Warren - 2/12/2012 10:41:41 PM

Looks to me like the part is made in each half of the mould.  Each part is then bonded together then held in the 2 part mould to align it while it sets.