By noble350 - 6/12/2013 8:24:44 PM				
            
                      
            Hi,I wonder what are the properties (tensile strength, ultimate strain, thickness, ect) of Carbon Fibre Tape Plain Weave 232g 25mm. Also what resin you recommend to be used with this tape
  Thanks
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Warren (Staff) - 6/13/2013 9:42:44 AM				
            
                      
            The datasheet for the graphil pyrophil tow used in its construction is here: Datasheet
  You can use the tape with any resin system suitable for carbon fibre.
           
		 | 			
		 
	
	
						
		 	
		
	 |