By shadowbows - 2/10/2012 9:33:51 PM

hi guys anyone got any idea as to wether you can make archery bow limbs useing 3mm PCV foam core and a facing of

195g carbon cloth ?

love to have a go i know that the big boys use a foam core but just cannot find out what it is hopfully someone can help me out ?
By shadowbows - 2/10/2012 10:29:34 PM

Joe, thanks its a start i have had some good results with maple cores and gordon composite Eglass a

GC-70-ULS:UNIDIRECTIONAL FIBERGLASS WITH 50/50 WOVEN INLAY

but i am having a problem working out a comparison between this and as to bending of ProFinish™ carbon 200g, 3k, 2/2 twill carbon fibre fabric

which in a bow limb = pounds pull. if this makes any scence. I am thinking that swapping glass for carbon

may have the same bending stiffness so equaling the same poundage but having better torshonal stability

and so an increase in speed ?

Suppose i will just have to go shopping and give it a try.