Talk Composites - The Forum for Advanced Composites

Oven curing an infusion while "wet"

http://www.talkcomposites.com/Topic6163.aspx

By jamesw - 5/21/2013 9:41:17 PM

I'm trying to speed up my infusion work process - normally when the resin infusion is complete, I turn off the vacuum. Then leave overnight, then post cure.... I could transfer to the oven straight after turning off vac - any suggested ramps for this to achieve fast cure and 60-70 degree post cure?

Thanks,
James
By jamesw - 5/23/2013 7:25:23 PM

Many thanks !