            I have been making CF-foam-CF sandwiches using the resin infusion method, which involves using a layer of peel-ply under the infusion mesh. This leaves my panels with one smooth side (against the tool surface) and a rough side (courtesy of the peel ply.) 
  Is it possible to replace the peel-ply with, say, Perforated Release Film (or similar) to give a smoother finish? I'm not looking for a perfectly smooth/glossy surface, just not a peel-ply finish.
  Would Perforated Release Film (as used in wet lay-ups) allow the resin to permiate through to the CF-foam-CF sandwich beneath or would you just end up sucking the majority of your resin into the catch pot?
  Any advice appreciated.
  Phil.
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By philiplardner - 2/14/2012 6:54:45 PM				
            
                      
            Thanks Matt - that's much as I suspected - at least your confirmation saves me from having to knock up a trial-and-error test piece :- ) 
  I think I'll live with the peel-ply finish as the alternative is more work than it's worth for a non-cosmetic piece!