My third infusion - and finally this one pulled straight from the mold and only needed a quick polish and trim to look like this!
Spraying GC50 into the mould with the G100 gel spray gun has transformed my pieces (I was pinhole free on infusion 2 but was having carbon exposed at the surface)
There has been a lot of discussion about problems brushing GC50 - I have to advise just getting the correct kit and spraying it...
By prsw
-
5/14/2013 5:52:02 PM
ok, to bad.
then I will hold on tight to the bottle I got.
Warren (Staff) (14/05/2013)
Acetone doesnt work on GC50 anymore. The formulation has changed slightly since our bonnet video was filmed.