By carbonfibreworks
-
5/10/2013 6:22:19 PM
Three pairs of frame guards destined for the IOM TT , made from carbon and diolen with epoxy resin and post cured. Moulds and final components by
carbonfibreworks@aol.com
weight ? 90 grams each
All materials from EC .
By carbonfibreworks
-
5/13/2013 9:52:46 PM
prsw (13/05/2013)
Nice, lets hope they never get tested for real.
Me too