By Czar - 5/1/2013 5:14:22 PM

I have no experience working with carbon fibre. I absolutely love the look of this stuff.could anyone advise me on where and how to get started?  I am very interested in making carbon fibre parts and objects. I know of no one in Canada that makes carbon fibre products.is there any online courses I could take?
By stuart321 - 5/1/2013 7:09:15 PM

The easycomposites videos are very good and then there are many other videos and guides on Youtube and similar.

I found an Australian has posted some really useful videos:  http://www.youtube.com/user/WJP004?feature=watch he doesn't do resin infusion but provides loads of practical advice on mould making, wet-layups and thinking round problems of making parts (I think he was a taxidermist (sp) previously so has some intresting moulds!).

HTH