Hello,

It`s nice to learn of this interesting forum, I´m working to get a carbon fiber part of 4mm thinkness, I will use Resin infusion starter kit and about 12-13 Carbon Fibre Cloth Fabric 3k 2/2 Twill 195gsm layers, but actually, I do not know how much is the maximum recomended number of layers per infusion. Could someone give me an advise?

Thank you very much.


By jdaero - 4/18/2013 4:53:47 PM

Great! It is a good new to know that only needs one infusion process. I will spend more time and cloth to get it, It is late to buy 12k 650g, however, now I know this for future projects.