Hello to everyone.
New to the forum but very interested in everything carbon fibre.
I do a lot of cycling and have a pair of full carbon wheels. To protect the braking surface there is a coat of clear resin just where the brake blocks come into contact with the wheel. Usually when this surface has worn out its time to replace the rims but is there anything stopping me from re-applying a coat of very high temp resin?
Any advice will be greatly appreciated.
By josh636b1h
-
4/20/2013 10:22:41 PM
Thank you both for the replies.
I will drop Camcoat an email and see if they can help in any way.