Just joined and wanted to introduce myself. My name is Brian Alley and I operate Carbon Fiber Composites in West Virginia. We specialize in infusion and double bag infusion of carbon fiber parts for experimental aircraft and now manufacture structural assemblies Out of Autoclave with advanced double bag process. I hope I have something to offer the forum from our shop experience and also wish to learn from the group to add quality to what we offer our customers. Looking forward to meeting the membership.

Brian Alley
3043954932
By fgayford - 4/1/2013 12:05:11 AM

w10n320wt (31/03/2013)
I'll look thru my photo's and see if I have a good example. In the mean time here is a link to the article that got me started infusing.

http://www.compositesworld.com/articles/double-bag-infusion-70-fiber-volume

Enjoy!
Very nice. I would like to know the wait saving. Perhaps I need to do a test.

Fred