Mold has come out ok, but I got a little carried away with the newplast around the edges to seal the item.
Problem I now have is that I cannot release the newplast from the mold.
Does anyone has a good nack for removing this...
By Joe
-
2/7/2012 7:18:59 PM
Hey Tango,
On the Unimold video from the EC staff, they did also give a go with some
EasyLease Mold Cleaner
.
But Warren is absolutely right too.