Talk Composites - The Forum for Advanced Composites

Yet another prepreg question

http://www.talkcomposites.com/Topic5521.aspx

By fgayford - 3/23/2013 9:39:53 PM

I am having fun with Easy Composites prepreg. (6 parts so far) The last one is without the vacuum pump running.

The only thing that I need to know is what is the trick to peeling off the plastic coatings? I have enough problems at the grocery store getting the plastic rip off bags opened. There has to be a technic to do this easier. Right now I am using twizzers and a large needle.

So whats the trick guys??????????????Cry

Fred

Even supreme beings don't know it all.
By Nick Igoe - 5/17/2013 12:27:29 PM

Form my F1 days we always had a can of freeze spray on hand, don't forget if your pre-preg is getting a little warm you can always put your mould and materials back into to the freezer whilst you have a coffee etc  to keep it just right, no point in trying to rush a master piece.

As for removing the backing, quick flick at one corner with a pointed scalpel always did the trick for me.