Hi,
I'm a newbie here
and just about to make the moulds for my car mirrors.
These have the potential to become a big seller in the Alfa Romeo community.
The housing made entirely out of cf...
...I was wondering...
should I use the epoxy putty or perhaps the Uni-mould system?
A number of at least 10 sets of the DTM mirrors is expected to shift.
Help please
By Warren (Staff)
-
3/20/2013 4:57:20 PM
Either will work fine for that small kind of part. The putty is easier and quicker to mould small objects with though.