By alebassa - 3/11/2013 11:42:16 AM
Hi, I just introduced myself, I'm new to composites world.. Just an easy questions...
If I have two pieces made of FG and I need to join them togheter side to side, like putting two papers on a table side to side, can I just put some more cf with resin on the joint, overlapping the two parts, or do I need to use adhesive?
|
By alebassa - 3/11/2013 1:30:34 PM
Oh yes! I know that a split mould would have been best, but it was just the second part I ever made so a split mould seemed too much to start with... and also at the beginning I thought to do it like the original (left, right, front)... I'm just learning!!
|
|