By brasco - 3/1/2013 7:24:30 AM				
            
                      
            going to make a part with FG for my first big piece.
  lets assume i have my mold made and my dry materials laid out-- this i have worked out
  i have my vacuum kit together(hoses,fittings etc)--this i can work out and get set up
  what goes where before it gets the final bag for sealing?--here i need suggestions  
  what materials go where and what are the properties of each material?
  i think i am talking about peel ply and then soric?  or is there another step?
 
  thanks everyone, i appreciate all your help.
 
  scott
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By brasco - 3/1/2013 5:15:52 PM				
            
                      
            hahahahahahaa will do !  i am sure i'll eff up a few pieces too.
           
		 | 			
		 
	
	
						
		 	
		
	 |