By brasco - 2/25/2013 1:45:39 AM

as for the filleting wax sold by easy composites--
is it ok to recycle it? or does it all go to hell with various mold release agents and other contaminants
as you try and use it over and over?
 i am going to order some in 2 weeks and i was wondering about this,  and if i should get 2 packages of it.

thanks


scott
By brasco - 2/26/2013 11:03:16 PM

thanks for the replies !