By brasco - 2/17/2013 6:12:52 PM

is wet sanding ok to do for dust control?
wet sanding has other good qualities too, like it makes your sandpaper last longer and doesnt clog the paper.


thanks guys


scott
By wozza - 2/18/2013 5:18:15 AM

I always wet sand. When doing CF by watching the colour of the water you know that if it turns grey/black then you have sanded through the resin and into the cloth. (easily done by the way)