I do not know very well pro finish carbon fiber....
So, Is it tacky?
By star.ace
-
2/20/2013 4:15:41 PM
FLD (15/02/2013)
No, its small blobs of cured resin so it holds the weave pattern better than unsupported fabric. Works well but has slightly less drape than unsupported fabric.
ok and thanks a lot!