By pedcrist - 2/15/2013 12:40:43 AM
Hi,
I´ve made a CF tube, but the High Shrink Tape made a few wrinkles on it(it was the first time that i used it), so i need to apply a coat of resin to cover the wrinkles.
This resin need to cure one week at 25ºC. To apply this coat, do i have to wait it fully cure, or can i apply it right now? (it already past about 36 hours)
Pedro
|
By pedcrist - 2/19/2013 3:14:15 PM
Ok.
Thanks to all.
Pedro
|
|