Talk Composites - The Forum for Advanced Composites

Looking for advice

http://www.talkcomposites.com/Topic4834.aspx

By RRE - 2/14/2013 1:08:38 AM

I need some advice. What would be the best way to make the below product out of carbon fiber? It needs to be perfectly round. I'm not sure you can make this perfectly round just using a dremel tool or something like it or am I missing something? Also, would you make this from a mould or would you make it off the back of this part? I think I prefer a mould but would like some other opinions. Also, should it be vacuum infused, or just wet lay up with vacuum bagging?

By RRE - 2/22/2013 1:44:12 AM

Its an aluminum dust cover for wheels. I have been doing some research since I posted this and found some prepreg that can be stored at 75F or less and still work. The instructions on the prepreg say you don't need an autoclave, and can get by with just an oven. I was thinking of ordering some and trying to make this part off the back of it and see how it works out.