Hi i am new to this forum.. but i already doing carbon part form easy composite...

Here are my second attempts on carbon Kevlar for 4G63 cover plug using vinyl ester resin using infusion technique learn form easy composite.http://www.talkcomposites.com/Uploads/Images/5ec353f1-742f-4f33-a9cc-b9be.jpghttp://www.talkcomposites.com/Uploads/Images/78dd4f7c-cc95-418e-bff6-89ee.jpg  
By TomDesign - 2/4/2013 9:39:39 PM

nice can you tell difference epoxy and your vinilyster? anyone anything about these resins?