By Warren - 1/31/2013 10:54:04 PM
This project was the first one i ever did. The moulds were made a few years ago:


I tried it wetlay and infusion and couldnt get either to work properly.
So instead i moved onto pre-preg. It was sooo much easier to lay up the part:
 that was the surface layer.
the next layer was then added:

The whole lot was then put in a vacuum bag ready to be cured:

Once cured they were trimmed:
 I am well happy with the finish! just a little sanding for smooth edges and it will be ready to fit!
|
By Warren - 2/1/2013 8:28:22 PM
lol at the tit reference.
They are satin finish as the original part and mould were. Carbon doesnt photograph very well.
|
|