By crud249 - 1/24/2013 12:07:55 PM
Hi,
I am very used to wet lay with polyester resin and epoxy resin infusions. I now need my wet lay parts to be stronger and stiffer so want to use epoxy wet lay resin. Could you tell me if the fast cure resin has a green time to trim the excess like polyester resin. I realise I may have to wait longer but I'm just not sure if it will trim the same as polyester?
Thanks in advance
Chris.
|
By crud249 - 1/24/2013 1:37:19 PM
Thanks Warren,
Thats great. Just wanted to confirm that it is trimable as with polyester. I have just ordered some fast EL2 resin from you to try.
Cheers, Chris.
|
|